Data sheet
Wieland-G07
Wieland-G07 is a medium-hard bearing material with good sliding and emergency running properties. Compared to other cast materials it is inexpensive. Used in the extension arms of mowing equipment, guide elements in hydraulic cylinders and in general mechanical engineering.
Composition (standard values)
Sn 7 %
Pb 7 %
Zn 4 %
Cu balance
Material designation
Wieland G07
EN 1982 : 1998
Max. load
Oscillating bearing up to 50 MPa
Types available
Machined bushings
Tube dimensions for machined bushings
Continuously cast OD up to 200 mm
above please enquire
Physical Properties (standad values)
Density [g/cm3] | 8.9 |
Coefficient of thermal expansion (20 - 300 °C) [10-6/K] | 18.5 |
Thermal conductivity [W/m*K] | 63 |
Modulus of elasticity (20 °C) [GPa] | 93 |
Mechanical properties (standard values)
Temper | |
Hardness [HB/HRB] | 150 (HRB 83) |
Tensile strength Rm [MPa] | 530 |
0.2 %-proof stress Rp0.2 [MPa] | 350 |
Elongation A5 [%] | 10 |
1 MPa = 1 N/mm2